COROLIT 12
CLASSIFICATION
DIN 8555 | DIN EN 14700
MF 20-50-CTZ | T Co 2-50-CTZ
CLASSIFICATIONGENERAL CHARACTERISTICS
This cobalt base-alloy is the toughest, with highest corrosion and thermal resistance of all cobalt-base alloys. The weld deposit is machinable and is used on components that are exposed to high temperatures, corrosion and impact stress, such as valve seats as well as components in the chemical industry. Work hardening up to 45 HRc.
APPLICATION
thermal shock resistant, abrasion, erosion, corrosion, cavitation at high temperature, bearing surfaces, chemical industry, hot shear blades, valves
Typical all weld metal analysis %:
C | Si | Mn | Cr | Co | W | Fe |
1,4 | 1,0 | 0,8 | 29,0 | Base | 8,0 | <3,0 |
TYPICAL ALL WELD METAL MECHANICAL PROPERTIES
Hardness: 45 - 48 HRc
PARAMETER
Measurement | Voltage | Amps |
1,2 | 20-24 | 150-200 |
1,6 | 22-26 | 180-240 |
2,0 | 25-27 | 220-260 |
2,4 | 25-27 | 260-300 |
2,8 | 26-28 | 280-340 |
Forms of delivery
"Coil BS 300" = 15 kg | "Coil BS 450" = 25 kg | Drums = 300 kg |
Corodur may change the chararcteristics of the wire without notice. Statements on composition an application are just for the applier's information. Statements on mechanical properties always refer to the all-weld-metal according to valid standards. We recommend the applier to check our products for their special application autonomously.