COROLIT 25

CLASSIFICATION

DIN 8555 | DIN EN 14700
MF 20-300-CKTZ | T Co 1-300-CKTZ

GENERAL CHARACTERISTICS

COROLIT 25 deposits a cobalt- based alloy with an austenitic structure. This alloy contains approximately 10,5% nickel for matrix stability during elevated temperature service. It is resistant to hot corrosion, impact, wear and extreme temperature shocks and oxidation. The alloy is machinable by hard faced tools. COROLIT 25 is used for gas turbine components, on steam and chemical valves and on equipment handling hot steel, such as tong bits, shear blades, pumps for high temperature liquids. It is suitable for use at temperatures up to 900 °C.

APPLICATION

Hot forging tools, aerospace industry, turbo charger buckets, parts subject to high operating temperatures in combination with all types of wear such as impact, pressure, corrosion, erosion.

Typical all weld metal analysis %:

C Si Mn Cr Ni Co W Fe
0,12 0,8 1,0 20,0 10,5 Base 15,0 <3,0

TYPICAL ALL WELD METAL MECHANICAL PROPERTIES

Hardness: 250 - 280 HB

PARAMETER

Measurement Voltage Amps
1,2 20-24 150-200
1,6 22-26 180-240
2,0 25-27 220-260
2,4 25-27 260-300
2,8 26-28 280-340


Forms of delivery

"Coil BS 300" = 15 kg "Coil BS 450" = 25 kg Drums = 300 kg

Corodur may change the chararcteristics of the wire without notice. Statements on composition an application are just for the applier's information. Statements on mechanical properties always refer to the all-weld-metal according to valid standards. We recommend the applier to check our products for their special application autonomously.