CORODUR® TS 625

CLASSIFICATION

T Ni 6625
T Ni Cr Mo- 3
2.4621

GENERAL CHARACTERISTICS

Suitable for joining and cladding stainless, heat resistant and cold tenacious steels as well as welding dissimilar materials for example low alloyed steels with Ni-base or Cu-base alloys The austenitic deposit is insensitive to hot-cracking and free of embrittlement at high as well as at low temperatures, non-scaling up to 1100° C, and cold tough down to –196° C. No diffusion of carbon into the weld metal at high temperatures. Used for service-temperatures of more than 300° C in chemical industry, petrochemical industry, glassworks, civil engineering, repairing and maintenance workshops.

APPLICATION

1.4558     2.4631     2.4605        2.4618       2.4619        2.4630
2.4641     2.4660     2.495          2.4816       2.4817        2.4851
2.4856     2.4858     1.5662        1.5680       1.5681        1.6907
1.6967     1.4876     1.4959        Alloy 800    Alloy 800HT

TYPICAL ALL WELD METAL ANALYSIS (%):

C Si Mn Cr Mo Nb Ni
0,02 0,3 0,4 21,0 9,0 3,4 Basis

TYPICAL ALL WELD METAL MECHANICAL PROPERTIES

Tensile strength Rm
N/mm²
Yield strength
Rp0,2 N/mm²
Elongation
A5 %
Impact strength
(J)
780 500 40 - 196 C°; 70

FORMS OF DELIVERY

Diameter / mm
Sales units
Shielding gas
1,2 BS 300 Argon + Co2
1,6 BS 300 Argon + Co2



PDF Factsheet