CORODUR® TS 625
CLASSIFICATION
T Ni 6625
T Ni Cr Mo- 3
2.4621
GENERAL CHARACTERISTICS
Suitable for joining and cladding stainless, heat resistant and cold tenacious steels as well as welding dissimilar materials for example low alloyed steels with Ni-base or Cu-base alloys The austenitic deposit is insensitive to hot-cracking and free of embrittlement at high as well as at low temperatures, non-scaling up to 1100° C, and cold tough down to –196° C. No diffusion of carbon into the weld metal at high temperatures. Used for service-temperatures of more than 300° C in chemical industry, petrochemical industry, glassworks, civil engineering, repairing and maintenance workshops.
APPLICATION
1.4558 2.4631 2.4605 2.4618 2.4619 2.4630
2.4641 2.4660 2.495 2.4816 2.4817 2.4851
2.4856 2.4858 1.5662 1.5680 1.5681 1.6907
1.6967 1.4876 1.4959 Alloy 800 Alloy 800HT
TYPICAL ALL WELD METAL ANALYSIS (%):
C | Si | Mn | Cr | Mo | Nb | Ni |
0,02 | 0,3 | 0,4 | 21,0 | 9,0 | 3,4 | Basis |
TYPICAL ALL WELD METAL MECHANICAL PROPERTIES
Tensile strength Rm N/mm² |
Yield strength Rp0,2 N/mm² |
Elongation A5 % |
Impact strength (J) |
780 | 500 | 40 | - 196 C°; 70 |
FORMS OF DELIVERY
Diameter / mm |
Sales units |
Shielding gas |
1,2 | BS 300 | Argon + Co2 |
1,6 | BS 300 | Argon + Co2 |